Logo — SPECTRA

SPECTRA / INVESTMENT POWDERS

TRIVEST

One investment.
More possibilities.

Reliable, everyday performance. A thin, creamy mix for detailed castings in yellow and white gold up to 18K, sterling silver, fine silver and bronze.

Calculate your mix ↓
TRIVEST — SPECTRA
  • 22.5 kg plastic-lined poly sacks
  • 22.5 kg ergonomic plastic drums
  • 45 kg heavy-duty reusable plastic drums
  • Reusable drums can also contain used investment.
TRIVEST – Versatility for your workshop — SPECTRA

THE TRIVEST DIFFERENCE

Versatility for
your workshop.

TRIVEST is a premium gypsum bonded investment for workshops that prefer one formula for multiple casting applications. Designed for gold up to 18K, it also supports complex designs in sterling silver, fine silver and bronze.

  1. Controlled expansion
  2. Smooth mixing
  3. Consistent results

PREPARE YOUR BATCH

Your mix.
Calculated.

Catalog range: 38–40%. Additional setting: 37%.

Choose your water ratio
kg

Enter the weight of dry powder.

WATER REQUIRED
0.38 liters

1 kg powder × 0.38 = water in liters
100 parts powder : 38 parts water

Water 21–24°CWorking time 8 min
  1. 01

    Weigh & prepare

    Measure the calculated water at 21–24°C and weigh your TRIVEST powder.

  2. 02

    Add powder to water

    Always add powder to the measured water, in that order.

  3. 03 · 4–5 MIN

    Mix under vacuum

    Mix and vacuum together for 4–5 minutes.

  4. 04 · 2 MIN

    Pour into the flask

    Fill the prepared flask within 2 minutes.

  5. 05 · 1 MIN

    Vacuum the flask

    Vacuum the filled flask for 1 minute.

  6. 06 · 90–120 MIN

    Leave undisturbed

    Allow the flask to stand for 90–120 minutes before burnout.

Choose your water ratio.

STANDARD BURNOUT CYCLE

Controlled heat.
Confident preparation.

13 hours to complete the peak-temperature hold.

The time under each temperature is the hold at that temperature.Swipe the chart to see the complete program →

TRIVEST standard burnout program Ramp to 150 degrees Celsius in 1 hour, hold 3 hours. Ramp to 370 in 1 hour, hold 2 hours. Ramp to 750 in 2 hours, hold 4 hours. Then cool to the required flask temperature for casting. The cooling segment is schematic; no cooling time or casting temperature is specified. 8006004002000°C01457913TIME IN HOURS 150 °C3 h370 °C2 h750 °C4 h
Injection wax
Target temperatureTime to reach targetHold at target
150 °C1 h3 h
370 °C1 h2 h
750 °C2 h4 h

Cooling: no fixed duration is specified; follow the temperature required by your casting process.

150°C → 370°C → 750°C. The dashed cooling segment is illustrative; the final temperature depends on your alloy and casting process.

YOUR NEXT CASTING

Let’s get the details right.

Discuss TRIVEST, your mixing process or your next order with our team.

LET’S TALK CASTING

Let’s talk about TRIVEST.

Product selection, processing questions or a new project — share a few details with our team.

chris@certus-int.com

Your inquiry will be sent to the CERTUS team.

Open in email app chris@certus-int.com

Choose your language

Select a language. You will stay on this page.

EnglishРусскийEspañolDeutsch简体中文ItalianoالعربيةBahasa Indonesiaहिन्दीTürkçePortuguês (Portugal)ไทยFrançaisاردوفارسیO‘zbekchaTiếng ViệtPortuguês (Brasil)

Thank you for your inquiry

Our team will use the email address you provided to get back to you. For anything else, you can also reach us directly.

chris@certus-int.com