Logo — SPECTRA

SPECTRA / INVESTMENT POWDERS

MOMENTUM

For larger non-ferrous
art designs & commercial parts.

Industrial-grade gypsum-bonded investment for non-ferrous metal components and complex commercial parts.

Calculate your mix ↓
MOMENTUM — SPECTRA
  • 22.5 kg plastic-lined poly sack
  • 1 metric ton heavy-duty bulk bag
MOMENTUM – From expressive forms. To engineered parts — SPECTRA
Industrial precision casting
MOMENTUM – From expressive forms. To engineered parts — SPECTRA
Atelier 80 Logo — SPECTRACasting by
Bronsgieterij Atelier 80

THE MOMENTUM DIFFERENCE

From expressive forms.
To engineered parts.

MOMENTUM is an industrial-grade gypsum bonded investment for non-ferrous casting. Its applications span sculpture, art forms, figurines, class rings and decorative pieces, as well as complex components for commercial use.

  1. For art and industry.

PREPARE YOUR BATCH

Your mix.
Calculated.

Water / powder ratio · 21–24°C

Choose your water ratio
kg

Enter the weight of dry powder.

WATER REQUIRED
0.34 liters

1 kg powder × 0.34 = water in liters

Water 21–24°CWorking time 11 min
  1. 01 · Prepare

    Weigh powder & water

    Measure the calculated water at 21–24°C and weigh the MOMENTUM powder.

  2. 02 · In this order

    Add powder to water

    Always add the powder to the measured water.

  3. 03 · 4–5 min

    Mix under vacuum

    Mix and vacuum together for 4–5 minutes.

  4. 04 · 3 min

    Pour into the flask

    Pour gently along the inside wall within 3 minutes. Cover the patterns by at least 2.5 cm (1″).

  5. 05 · 3 min

    Vacuum the flask

    Vacuum the filled flask for 3 minutes.

  6. 06 · 180–240 min

    Allow to stand

    Leave undisturbed in a vibration-free area for 180–240 minutes before burnout.

After the 11-minute working sequence, stand the flask undisturbed in a vibration-free area for 180–240 minutes. Cover the top of the patterns with at least 2.5 cm (1″) of investment.

INJECTION-WAX BURNOUT CYCLE

Controlled burnout.
Prepared for casting.

Injection-wax reference curve · 18 hours before cooling

The time under each temperature is the hold at that temperature.Swipe the chart to see the complete program →

MOMENTUM injection-wax reference burnout curveCatalog reference chart: ramp to 149 degrees Celsius over 1 hour, hold 4 hours. Ramp to 250 over 1 hour, hold 2 hours. Ramp to 730 over 5 hours, hold 5 hours. Eighteen hours before cooling. Cool to the required flask temperature for casting; cooling is schematic. The separate written steam and dry instructions below specify a 732-degree peak, variable hold ranges and a final stabilization hold.0200400600800015681318°CTIME IN HOURS149 °C4 h250 °C2 h730 °C5 h
Reference curve
Target temperatureTime to reach targetHold at target
149 °C1 h4 h
250 °C1 h2 h
730 °C5 h5 h

Cooling: no fixed duration is specified; follow the temperature required by your casting process.

Reference chart: 149°C → 250°C → 730°C. The written procedures below specify 732°C, with variable holds. Burnout time may vary with flask size; the cooling line is illustrative.

Detailed catalog instructions

Steam or dry dewaxing.

Written procedure: 732°C peak.
Use the timings and conditions below as one complete sequence.

Steam dewaxing

Use steam only long enough to remove the bulk of the wax. Excessive exposure can erode the investment surface. Immediately transfer the flask to the oven preheated to 149°C; do not let it cool between steam dewaxing and burnout.

Dry dewaxing

Place the flask directly into an oven preheated to 149°C. At the peak hold, ensure all carbon residue from the wax has been eliminated before lowering to the casting temperature.

Written MOMENTUM burnout sequence after the selected dewaxing preparation
StageTemperature / actionTime / condition
01 / Hold149°C in the preheated oven4–6 hours
02 / Raise & holdIncrease to 250°CHold for 2 hours
03 / RampIncrease to 732°C66–93°C per hour
04 / Peak hold732°C4–5 hours; for dry burnout, until all wax carbon is eliminated
05 / CoolLower to the required mold temperatureAccording to the alloy and casting process
06 / StabilizeHold at casting mold temperature2 hours; for dry burnout, longer if needed to stabilize throughout the mold

For casting aluminum204–282°C

Bronze & most copper-based alloys427–538°C

These are mold temperatures for casting, not metal pouring temperatures. Once the mold temperature has stabilized throughout, the mold is ready to cast.

Written procedure: 149°C → 250°C has no specified ramp duration. For 250°C → 732°C at 66–93°C/h, the calculated ramp time is approximately 5 h 11 min–7 h 18 min (311–438 min). These timings are separate from the reference curve.

YOUR NEXT CASTING

Let’s get the details right.

Discuss MOMENTUM, your mixing process or your next order with our team.

LET’S TALK CASTING

Let’s talk about MOMENTUM.

Product selection, processing questions or a new project — share a few details with our team.

chris@certus-int.com

Your inquiry will be sent to the CERTUS team.

Open in email app chris@certus-int.com

Choose your language

Select a language. You will stay on this page.

EnglishРусскийEspañolDeutsch简体中文ItalianoالعربيةBahasa Indonesiaहिन्दीTürkçePortuguês (Portugal)ไทยFrançaisاردوفارسیO‘zbekchaTiếng ViệtPortuguês (Brasil)

Thank you for your inquiry

Our team will use the email address you provided to get back to you. For anything else, you can also reach us directly.

chris@certus-int.com