A non-foamed investment molding plaster developed for aluminum alloy casting. Engineered for the precise, complex tread patterns of tire vulcanization molds.

Calculate your mix ↓
MOMENTUM TIRE — SPECTRA
  • 22.5 kg plastic-lined poly sack
  • 1 metric ton heavy-duty bulk bag
MOMENTUM TIRE – Every groove. Every detail — SPECTRA
Aluminum alloys · Tire vulcanization molds · Complex tread patterns

THE MOMENTUM TIRE DIFFERENCE

Every groove.
Every detail.

MOMENTUM TIRE is a non-foamed, gypsum bonded investment molding plaster developed for casting aluminum alloys for tire mold production. It reproduces intricate tread configurations for molds used in tire vulcanization.

  1. Precision in every tread.
  2. A smoother casting surface.
  3. Consistency through production.

PREPARE YOUR BATCH

Your mix.
Calculated.

Method-specific water quantities · 21–24°C

kg

Enter the weight of dry powder.

WATER REQUIRED
0.5 liters

1 kg powder × 0.50 = water in liters

Water 21–24°CWorking time 11 min
  1. 01 · Prepare

    Weigh powder & water

    Measure the calculated water at 21–24°C and weigh the MOMENTUM TIRE powder.

  2. 02 · In this order

    Add powder to water

    Add the powder to the measured water.

  3. 03 · 4–5 min

    Mix under vacuum

    Mix and vacuum together for 4–5 minutes.

  4. 04 · 3 min

    Pour into the mold

    Pour the mixed investment into the mold flask over 3 minutes.

  5. 05 · 3 min

    Vacuum the mold

    Vacuum the filled mold flask for 3 minutes.

  6. 06 · 120–150 min

    Allow to stand

    Leave undisturbed for 120–150 minutes before burnout.

After the 11-minute working sequence, leave the filled mold undisturbed for 120–150 minutes before burnout. Measure accurately: a 1% increase in powder can shorten working time by approximately 30 seconds.

RECOMMENDED TIRE-MOLD BURNOUT CYCLE

The tire-mold cycle.
Every stage in view.

Two plateaus · 24 hours before cooling.
Burnout time may vary with mold size.

The time under each temperature is the hold at that temperature.Swipe the chart to see the complete program →

MOMENTUM TIRE catalog burnout cycleRamp to 150 degrees Celsius over 2 hours, hold for 7 hours. Ramp to 295 degrees over 5 hours, hold for 10 hours. Total: 24 hours before cooling. Cool to the required flask temperature for casting. Cooling duration and target temperature are not specified; the dashed cooling segment is schematic. Vertical scale: zero to 350 degrees Celsius.0501001502002503003500291424°CTIME IN HOURS150 °C7 h295 °C10 h
Injection wax
Target temperatureTime to reach targetHold at target
150 °C2 h7 h
295 °C5 h10 h

Cooling: no fixed duration is specified; follow the temperature required by your casting process.

150°C → 295°C · 24 hours before cooling. Lower to the required casting temperature; the dashed line is schematic and specifies neither a fixed cooling time nor a target temperature.

YOUR NEXT CASTING

Let’s get the details right.

Discuss MOMENTUM TIRE, your tire mold process or your next order with our team.

LET’S TALK CASTING

Let’s talk about MOMENTUM TIRE.

Product selection, processing questions or a new project — share a few details with our team.

chris@certus-int.com

Your inquiry will be sent to the CERTUS team.

Open in email app chris@certus-int.com

Choose your language

Select a language. You will stay on this page.

EnglishРусскийEspañolDeutsch简体中文ItalianoالعربيةBahasa Indonesiaहिन्दीTürkçePortuguês (Portugal)ไทยFrançaisاردوفارسیO‘zbekchaTiếng ViệtPortuguês (Brasil)

Thank you for your inquiry

Our team will use the email address you provided to get back to you. For anything else, you can also reach us directly.

chris@certus-int.com